Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
DuPont Bynel® 3030 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA837091 Linear Medium Density Polyethylene ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for extrusion and injection-blow molding. An antioxidant had been added to ensure thermal stability. Pro.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 110-1327 LMDPE Rotational Molding Resin Description: ICORENE 110-1327 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 110-3561 LMDPE Rotational Molding Resin Description: ICORENE 110-3561 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1327 LMDPE Rotational Molding Resin Description: ICORENE 115-1327 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792-91 |
Micropol Microcene MC121 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792 |
Micropol Microlin ML21 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183/ISO 1872-2B |
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183/ISO 1872-2B |
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | Base Resin; ASTM D1505 |
Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding Borecene Compact RM8346 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | Base Resin; ASTM D1505 |
Borealis Borecene Compact™ RM8346RC Black Linear Polyethylene for Rotational Molding Borecene Compact RM8346RC is a third generation linear medium density black polyethylene for rotational molding. Borecene RM8346RC is a special grade, which has passed rigorous tests and can be con.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Borealis Borecene™ RM8342 Linear Polyethylene for Rotational Molding Borecene RM8342 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Borealis Borecene™ RM8343 Linear Polyethylene for Rotational Molding Borecene RM8343 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Borealis Borecene™ RM8343PL Linear Polyethylene for Rotational Molding Borecene RM8343PL is plasma treated linear medium density natural polyethylene for rotational molding with improved adhesion properties. The material is plasma treated to change the chemical struct.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 410 Ethylene Vinyl Acetate DuPont™ Elvax® 410 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 410 resins can be used for the following applications: adhesives, sealants.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | Result |
Westlake Plastics Lennite® GUR1050 (Type II) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ISO 1183 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 705.MJ Molding, extrusion and compounding resin Escorene Ultra LD 705.MJ is a fraction melt index, 13.3 wt% vinyl acetate copolymer suitable for use in making blow molded articles, extruded profiles and compounds.Information provided by ExxonMobi.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 151HR Low Density Polyethylene Resin Product Description: LD 151 series LDPE grades offer an excellent combination of high clarity with high stiffness. Several additive packages are available according to the required surface propertie.. |
|||
Density | 0.934 g/cc | 0.0337 lb/in³ | ASTM-D1505 |
Braskem CN8092 EVA Molding Copolymer CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i.. |