Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | <= 0.930 g/cc | <= 0.0336 lb/in³ | ISO 1183 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | STN 64 0111 |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
PolyOne OnFlex™ V 3085A-S0098 Thermoplastic Elastomer (TPE) OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D 792 |
NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin IFs730-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900 UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, .. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
LyondellBasell Montell HB320CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | MBA Method |
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D1475-85 |
Lord Adhesives Aeroglaze® Z302 Absorptive Polyurethane Aeroglaze® Z302 absorptive polyurethane is primarily for application to substrates used in space operations. These operations include those where coatings must exhibit low outgassing characterist.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
Lushan L-5R Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792B |
LyondellBasell Astryn BA35H Polypropylene Copolymer, Flame Retardant Key Features: conventional melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colora.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | |
Solvay RHODASURF® LA 42 Surfactant Identification: ETHOXYLATED FATTY ALCOHOLCAS: 68439 – 50 – 9Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America .. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM-D1505 |
Westlake EB171 MDPE Medium Density Polyethylene Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP K 0200 V2 Flame Retardant Polypropylene PP copolymer extrusion gradeFlame retardant class V2, PBDE free, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ LNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high stiffness, high gloss, low discoloration and good detergent resistance for large electrical appliances such as washing machi.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | |
Dow SiLK™ Y 120 Semiconductor Dielectric Resin SiLK™ Y 120 has an average pore size of < 2nm and a range of 1-3 nm, porous SiLK™ resins enables continuous Tantulum PVD barriers for 65 nm technology and beyond. Information provided by Dow |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | |
Dow SiLK™ Y 250 Semiconductor Dielectric Resin SiLK™ Y 250 has an average pore size of < 2nm and a range of 1-3 nm, porous SiLK™ resins enables continuous Tantulum PVD barriers for 65 nm technology and beyond. Information provided by Dow |
|||
Density | 0.930 g/cc @Temperature 23.0 °C |
0.0336 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula.. |
|||
Density | 0.930 g/cc @Temperature 23.0 °C |
0.0336 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 320 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 320 is particularly.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | |
3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ISO 1183 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Huntsman PE1076 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792 |
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting
(discontinued **)&l 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Density | 0.930 g/cc | 0.0336 lb/in³ | ASTM D792-ISO 1183, ASTM D1505 |
DuPont Elvax® 760Q Ethylene Vinyl Acetate DuPont™ Elvax® 760W is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 760Q resins can be used for the following applicati.. |