Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Network Polymers NPP 30-3000 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
M. Holland Company LD225 LDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, High Clarity, High Gloss, Heat Sealable, Good Processability, Medium SlipUses: FilmProcessing Method: Blown FilmInformation pro.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1558 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Global TPO-45D TPO Grade Data provided by Global Polymers Corporation. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Density | 0.925 - 0.950 g/cc | 0.0334 - 0.0343 lb/in³ | ASTM D1505 |
Micropol Microlink XL Crosslinkable Polyethylene Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ISO 1183 |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ISO 1183 |
Borealis Steripeel™ WE150CF PO Compound for Sterilizable Peelable Film Applications Steripeel WE150CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WE150CF is suitable for.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Westlake Hifor Xtreme SC74849 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74849 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock, and polymer processing aid.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D-1505 |
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Melt |
Covestro Desmopan® DP 6065A Polyurethane injection molding gradefree from plasticizersvery good hydrolysis and microbial resistancevery short cycle timesApplicationhard - soft systemsShoe solesPreprocessingMax. Water content |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LD 313.NF Blown Film Resin LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 158BW Low Density Polyethylene Resin Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D4883 |
ExxonMobil LL 6100.17 Injection Molding Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1201XV Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1201 series are LLDPE grades, offering excellent combination of stiffness and optical properties (when blended with 10-20% LDPE) Availability: Africa & Middle East, Asia Paci.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 5001.09 Linear Low Density Polyethylene Resin Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending .. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D-1505 |
Bapolene® 2292 Polyethylene Film Grade Bapolene 2292 is a butene linear low density polyethylene copolymer designed to provide a combination of toughness and stiffness and complies with FDA 21 CFR177.1520.Applications: Closures, lids, an.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | |
Arkema Group Evatane® 1005 VN 2 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process.Applications Grade for transparent and resistant film production. Examples: curtain stretch, coextrusion, stretch hood.ISO data provided by the ma.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin
(discontinued **) Good processability, Excellent impact resistance, Excellent flexibility and freedom from warpageApplications: Automotive splash-guards, Large containers, Closures and lids for food applicationsAddit.. |