Chevron Phillips KN 226B LDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips KN 226B LDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Moderate ESCRApplications:Housewares, Personal Care Products, Luggage HandlesData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 24.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Modulus 0.186 GPa
27.0 ksi
3 pt. secant; ASTM D790
0.269 GPa
39.0 ksi
3 pt. Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746