Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
load density; ASTM D1505
SABIC 324CN Linear Low Density Polyethylene for Wire & Cable
Product Description: 324CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin
Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D 792
NOVA Chemicals Novapol® LM-0724-A LDPE Injection Molding Resin
LM-0724-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin  (discontinued **)
Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792
NOVA Chemicals Novapol® LF-Y824-C LDPE Clarity Film Resin  (discontinued **)
Features: High optical clarityExcellent processabilityExcellent shrink film characteristics Applications: High clarity shrink filmProduce and bakery filmTextile packaging filmInformation provided by..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792
DuPont Bynel® 3048 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Huntsman PE1356 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Huntsman PE 1402 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
LyondellBasell Plexar® PX3060 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and ..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
ApplicationsPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copo..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5069 400 Micron LLDPE Powder
Description: ICOFLO 510-5069 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
ICO Polymers ICOFLOâ„¢ 510-5071 800 Micron LLDPE Powder
Description: ICOFLO 510-5071 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Density 0.924 g/cc
0.0334 lb/in³
ISO 1183
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate
Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
UBE F022SE Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792 - ISO 1183
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Westlake EF403 Low Density Polyethylene
WESTLAKE polyethylene EF403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent skrinkability, and has very good optic..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Westlake EF403 Low Density Polyethylene
WESTLAKE polyethylene EB403 is a fractional melt low-density formulation suggested for use in clarity shrink applications. This LDPE formula exhibits excellent shrinkability, and has very good optic..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Westlake LF2018 Hexene Linear Low Density Polyethylene
Westlake LF2018 is a hexene LLDPE suitable for heavy duty films and shipping sacks. This material has increased stiffness, and can be blended with LDPE for strength property enhancements..Applicatio..
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil Method
ExxonMobil LD 306.75 High Clarity, High Impact Film Resin
LD 306 Series films exhibit superior impact strength and heat sealability. Applications include food packaging and frozen food packaging.Information provided by ExxonMobil Chemical
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil Method
ExxonMobil LD 334.57 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin
Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according..
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
ExxonMobil LDPE LD 653 Low Density Polyethylene Resin (European Grade)
Product Description: LD 653 is an easy flowing LDPE grade with medium stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: ..
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 6101XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D792
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7144 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as large industrial containers and trash cans. Information provide..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Huntsman PE2067 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: High flow resin, provides excellent gloss and surface characteristics, and minimum cycle time.Applications: Injection molding: lids.FDA Notes: Conforms to FDA..
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Reliance Industries Reclair M24300 Polyethylene
High flow Linear Low Density Polyethylene grade. Reclair M24300 is butene comonomer based, with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, good fluidity, ..
Copyright © lookpolymers.com All Rights Reserved