Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D 792 |
NOVA Chemicals Novapol® LF-0718-A-INJECTION LDPE Injection Molding Resin LF-0718-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. LF-0718-A is subj.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3301.34 Premium High Strength Film Resin
(discontinued **) LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Density | 0.917 - 0.966 g/cc | 0.0331 - 0.0349 lb/in³ | Average value: 0.951 g/cc Grade Count:156 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-279 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-276 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.921 g/cc | 0.0331 - 0.0333 lb/in³ | |
Kazanorgsintez 15813-020 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 162-280 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 g/cc @Temperature 20.0 °C |
0.0331 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PM Propylene glycol methyl ether Available in electronic grade.Information provided by Lyondell. |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-278 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.980 g/cc | 0.0331 - 0.0354 lb/in³ | ASTM D792 |
Plastic Lumber from the Plastic Lumber Co. Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake EM1550AA Low Density Polyethylene WESTLAKE low-density polyethylene EM1550 is a low-density formulation used for injection molding applications.Application/UsesFlexible medicalLidsMedicalFDA: This material complies with FDA regulati.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Westlake Tymax™ GT1057 Anhydride Modified Acrylate Copolymer Product Description: Westlake GT1057 is an anhydride modified low density polyethylene designed as an extrusion coating and laminating tie-layer. Westlake GT1057 provides excellent adhesion to pol.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505-60T |
Chevron Phillips MarFlex® 1019 Extrusion Coating Resin Resin Type: Very High Speed at Low Coating WeightsCharacteristics: Excellent Processability, Process at Lower Temperature, High Temperature Stability, Excellent Draw Down ResinApplications:Food Pack.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: HousewaresTamper evident, snap-on capsWine bottle sleeve capsInfo.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: Large housewaresTamper evident, snap-on capsFeminine hygiene appl.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ExxonMobil NTX™ NTX 095 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ExxonMobil NTX™ NTX 150 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | |
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | |
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | |
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM-D792 |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin
(discontinued **) Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Eastman D4042-P Polyethylene
(discontinued **) D4042-P is a low density resin designed for applications such as sugar pouches and freezer wrap, where high coating speeds and good drawdown are required. The combination of high melt index and low.. |