Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.980 g/cc | 0.0330 - 0.0354 lb/in³ | Average value: 0.945 g/cc Grade Count:71 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
Silon Tabond 3045 Adhesive Resin TABOND 3045 is LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Str.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Appeel® 45D747 Polyolefin Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade) Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D792 |
Dow ELITE™ 5500G Enhanced Polyethylene Resin ™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te.. |
|||
Density | 0.914 g/cc @Temperature 23.0 °C |
0.0330 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18360 Maleic Anhydride Modified Polyethylene OREVAC® 18360 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.914 g/cc @Temperature 0.000 °C |
0.0330 lb/in³ @Temperature 32.0 °F |
|
Akzo Nobel Trigonox® 121 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylates and methacrylates.Information provided by Akzo Nobel Polymer Chemicals. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
BASF Lupragen® N 400 Trimethylamineoethylethanolamine Formula: C7H18N2OCAS: 2212-32-0Description: Trimethylaminoethylethanolamine is a colorless to light yellow liquid, with an amine-like odor. It is miscible with water and other organic solvents.Syno.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
BASF N-Ethylethanolamine Formula: C4H11NOCAS: 110-73-6Description: N-Ethylethanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: EEA, 2-Ethylaminoethanol, 2-(Ethylamino)etha.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
ConocoPhillips 32 Spectrum Cutting Oil Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica.. |