Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® FP112-A Octene VLDPE Film Resin Features: Low seal initiation temperatureHigh toughnessVery good optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Low gel Applications: Sealant and lamination film for food packagi.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil Method |
ExxonMobil Exceed™ 1012CA Film Resin
(discontinued **) Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene 12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
LyondellBasell Hostacomâ„¢ BA742EC Polypropylene Copolymer Description: Hostacomâ„¢ BA742EC low melt flow, 1,200 MPa flexural modulus, precolored, extrusion grade polypropylene copolymer has a good balance of strength, stiffness, impact resistance and pr.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Silon Tabond 2004 Adhesive Resin TABOND 2004 is a copolymer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Silon Tabond 3032 Adhesive Resin Tabond 3032 is a chemically modified LDPE / LLDPE. Its functional groups improve considerably the bonding between polar polymers, for film applications.Characteristics: • Strong adhesion to PA .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil Method |
ExxonMobil EXXCO™ Exxco 012 w/20% LDPE Enhanced Performance Extrusion Coating Resin Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal stre.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA reg.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D792 |
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Dow ATTANE™ 4206 Ultra Low Density Polyethylene, Impact Modifier Grade ATTANE® 4206 copolymer is an ultra low density polyethylene that offers excellent performance as an impact modifier for durable molded parts. It provides excellent impact and rigidity improvements .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Dow ATTANE™ 4401 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4401 copolymer is an ultra low density polyethylene having high tear strength and impact resistance. It is designed for use in industrial/consumer film applications, either as high performa.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
Dow ATTANE™ 4601 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4601 copolymer is an ultra low density polyethylene blown film extrusion grade having high impact resistance and tear strength combined with improved softness, designed for use in medical p.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes.. |
|||
Density | 0.912 g/cc @Temperature 23.0 °C |
0.0329 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene OREVAC® 18365 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D1505 |
Arkema Group Orevac® 18302 Maleic Anhydride modified LLDPE Orevac® 18302 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers.Information provided by Arke.. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | |
ConocoPhillips Inca® 680 Oil, AGMA No. 8 Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Density | 0.912 - 1.86 g/cc | 0.0329 - 0.0672 lb/in³ | Average value: 0.993 g/cc Grade Count:32 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ASTM D1505 |
PolyOne Syncure™ S1042A Polyethylene, Crosslinked (XLPE) Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Deformation, and Gel measured on a 95 phr S1042A / 5 phr S1000B system; and cured .. |
|||
Density | 0.912 g/cc | 0.0329 lb/in³ | ExxonMobil Method |
ExxonMobil EXXCO™ Exxco 012 w/40% LDPE Enhanced Performance Extrusion Coating Resin Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal stre.. |