Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Network Polymers NPP 25-1011B Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH042V Polypropylene, Homopolymer, Extrusion, Sheet COPYLENE™ CH042V is a polypropylene homopolymer resin often used in extrusion applications. Replacement alternative to Pro-fax® HL561KInformation provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer COPYLENE® CR020CL is a random copolymer formulated with advanced clarifier technology and with antistat and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated COPYLENE™ CR120LN is a random copolymer nucleated and with antistat for good mold release in injection molding applications. Applications: Containers, Closures, HousewaresInformation provided by P.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR350CL Polypropylene, Random Copolymer, Clarified, Lubricated COPYLENE™ CR350CL is a clarified, easy molding high melt flow polypropylene random copolymer resin with good see-through and contact clarity in injection molding applications. Applications: Housewa.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR350CS-01 Polypropylene Random Copolymer COPYLENE® CR350CS-01 is a clarified, reactor grade, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release for larger ar.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation pro.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020-03 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applicationsApplications: Bags & Pouches, Raffia/Tapes/Strapping, Peelabl.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020S Polypropylene, Homopolymer, BOPP COPYLENE™ CH020S is a polypropylene homopolymer resin typically used by customers for BOPP (biaxially oriented polypropylene) Applications: Film ExtrusionInformation provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP COPYLENE™ CH034, a polypropylene homopolymer resin, is designed for the production of biaxially oriented polypropylene films (BOPP). Potential uses include metalized film applications, (either dire.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH050 Polypropylene, Homopolymer, Cast Film BOPP COPYLENE™ CH050 is a polypropylene controlled rheology homopolymer resin designed for Cast Film BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches, Pe.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH085S Polypropylene, Homopolymer, Cast Film, Slip COPYLENE™ CH085S is a controlled rheology polypropylene homopolymer resin containing slip additive. COPYLENE™ CH085S is used in injection molding and cast film extrusion applications. Applications.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM200LN Polypropylene Impact Copolymer COPYLENE™ CM200LN has a superior balance of stiffness and impact strength. The high melt flow allows for quick filling of molds and the antistat and nucleation facilitates fast cycle times.Applicat.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM200LN-02 Polypropylene Impact Copolymer COPYLENE™ CM200LN-02 is specially designed for injection molding applications where an excellent balance of stiffness/impact and good cycle times are required.Applications: Injection molding applic.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
LyondellBasell Pro-faxâ„¢ SC973 Polypropylene Copolymer Description: Pro-faxâ„¢ Ultra SC973 fully formulated (antistatic, nucleated, slip modified), very high melt flow, impact polypropylene reactor copolymer resin is designed for injection molding ap.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Mitsui EXCEREXâ„¢ 48070B(T) Polymer Processing Aid EXCEREXâ„¢ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREXâ„¢ gains in a number of ares simultaneously, including faster processing speeds.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/2-HP UV Polyolefin Catalyst CT/2-HP UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® and Polidiemme® ser.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis BE170MO Polypropylene Copolymer BE170MO is a heterophasic copolymer. This grade is characterized by high impact strength, high stiffness and good flow properties. This grade contains additives providing low taste and odor as well.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis RB607MO Polypropylene Random Copolymer RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications Product Description: Exact 0230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for both monolayer and multilayer co-extruded cast .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Dow AFFINITY™ PT 1450 Polyolefin Plastomer AFFINITY® PT 1450 polyolefin plastomer for extrusion coated packaging is an ethylene alpha olefin resin for monolayer and coextrusion coating that offers excellent low temperature seal initiation, .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem PRA 0852 RACO Random Polypropylene Copolymer PRA 0852 is a medium melt flow rate random copolymer with slip and antiblocking agents. It is suitable for blown and cast film extrusion. PRA 0852 has excellent optical properties and good processab.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem Prisma 2400 RACO Random Polypropylene Copolymer Prisma 2400 is a high melt flow rate random copolymer. This product is designed for the ISBM (Injection Stretch Blow Molding) process and offers low taste/odor. It can also be used in the blow moldi.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH034EV Polypropylene, Homopolymer, Fiber, Tape, UV COPYLENE™ CH034EV is a polypropylene homopolymer resin designed for fiber applications. Applications: Filament Yarn, Geotextile & agriculture. Equivalent to Pro-fax® HL348JInformation provided by .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer CM090L is a high impact copolymer with antistat and is specially designed to excel in injection molding processes for consumer products.Applications: Injection MoldingInformation provided by Phillip.. |