Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.240 g/cc | 0.00867 lb/in³ | ±10%; ASTM D3574A |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | ±10%; ASTM D3574A |
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | ±10%; ASTM D3574A |
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 15 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Zircar Ceramics Uniform A1 Alumina-Silica Insulation ZIRCAR Alumina-Silica Insulation Type "UNIFORM A" is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.240 g/cc | 0.00868 lb/in³ | |
Hexcel® HexWeb® HDC-G-327 - 3/16 - 15.0 (R2) Heavy Density Core Designation: Material-Cell Size (inches)-DensityHexWeb® HDC is a fabric reinforced honeycomb, typically made from either fiberglass or carbon prepreg. A thermosetting node adhesive is used with eit.. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 - 0.260 g/cc | 0.00867 - 0.00939 lb/in³ | Free Density |
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12036 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
3M 12030 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.240 g/cc | 0.00867 lb/in³ | |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |