Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Durafoam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.240 g/cc
0.00868 lb/in³
ASTM D1056
Water Absorption <= 5.0 %
<= 5.0 %
Weight change; ASTM D1056
Mechanical Properties Metric English Comments
Tensile Strength 0.621 MPa
90.0 psi
Die A; ASTM D412
Elongation at Break 175 %
175 %
Die A; ASTM D412
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
Deflection @ 25%; ASTM D1056
Tear Strength 3.51 kN/m
20.0 pli
Die C; ASTM D624
Compression Set <= 25 %
<= 25 %
ASTM D1056
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -40.0 °C
-40.0 °F
Minimum Service Temperature, Air 149 °C
300 °F
325 °C
617 °F
Intermittent
Descriptive Properties Value Comments
Color Black
Fluid Immersion <50%
(7 days at 73.4°F) ASTM Ref. Fuel B, Weight Change, ASTM-D-1056
Resilience 0.3
ASTM D2632