Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 3000 AE Expandable Polystyrene, Standard Flame Retardant Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 AE is: Molding, Vacuum.Specific characteristics: DIN.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
NOVA Chemicals EPS 33MAHD Modified Expandable Polystyrene Applications: Insulation, board stockInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS 33MC Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
NOVA Chemicals EPS 33MC Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS 34RB Regular Expandable Polystyrene Applications: PackagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
NOVA Chemicals EPS 34RB Regular Expandable Polystyrene Applications: PackagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS 34RC Regular Expandable Polystyrene Applications: PackagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Batch Expansion |
NOVA Chemicals EPS 35MB Modified Expandable Polystyrene Applications: Fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS M97BC Low Volatile/Low Pentane Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0160 g/cc | >= 0.000579 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS R244C Expandable Polystyrene Resin Applications Thermal and Regular PackagingInformation provided by NOVA Chemicals |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **) Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **) Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova Styrocell® M442C Expandable Polystyrene A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and convent.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | 1.2 minute residence time pre-expander |
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | 2 minute residence time pre-expander |
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | 75 rpm |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-301 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Density | 0.0160 g/cc | 0.000579 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 3/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0160 - 0.0480 g/cc | 0.000578 - 0.00173 lb/in³ | |
BASF Styropor® BF 327 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Density | 0.0160 g/cc | 0.000579 lb/in³ | Free Rise Density, 5% H<sub>2</sub>O |
ACC EP LS EPI Engineered Polymers Leak Stop MDI EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will soli.. |