Material Notes:
Sparkle Silver® 6246-AR has a high degree of flake orientation in coatings. It offers a rich, smooth, silver finish with excellent distinctiveness of image (D.O.I.) and gloss, yet it also has an unexpectedly deep flop.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Bulk Factor 0.083
0.083
Volatiles 38 %
38 %
Particle Size 13 µm
13 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.01% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash