Material Notes:
LED-2314AR is manufactured by incorporating a small amount of Teflonâ„¢ with a coated or treated aluminum pigment, and then, through further processing, is provided in a dry, non-dusting form. LED-2314AR is a polymer treated, fine, non-leafing, silver dollar lenticular aluminum pigment.Applications: Powder Coatings
Physical Properties Metric English Comments
Volatiles 0.60 %
0.60 %
Particle Size 13 µm
13 µm
Before dedusting
Descriptive Properties Value Comments
% Carrier 0.01
Before dedusting
Category Non-leafing