Silberline ET 2018 Metallescent

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline ET 2018 Metallescent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Metallescent pigments for plastics are designed to produce a soft diffuse appearance similar to the effect obtained by pearlescent mica pigments. Metallescent pigments produce their effect at very low loading levels and are therefore cost effective. The metallescent effect is best achieved by combining the metallescent pigment with transparent pigments or dyes.Applications: Plastics
Physical Properties Metric English Comments
Particle Size 11 µm
11 µm
Descriptive Properties Value Comments
% Carrier 60
Carrier Polyethylene Wax