Shin-Etsu Silicones KEP-12 Silicone additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KEP-12 Silicone additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KEP12 is an additive which can be used in most of the silicone products to improve heat stability.Product Features: Improve thermal stability and compression set.Excellent dispersion.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.66 g/cc
1.66 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
Tensile Strength at Break 10.7 MPa
1550 psi
Descriptive Properties Value Comments
Cure Agent DMBPH
DMPH
Cure Type Post Cure