Material Notes:
NANOCYL™ NC7000 Series, thin multi-wall carbon nanotubes, are produced via the catalytic carbon vapor deposition (CCVD) process.These carbon nanotubes are unique and prized world-wide because their small size and high aspect ratio (>150) lets them form a network of conductivity at a very low concentration. A primary interest is in applications requiring low electrical percolation threshold such as high-performance electrostatic dissipative plastics or coatings.During their production, Nanocyl uses exclusive catalysts that make the Nanocyl™ NC7000 the most electrically conductive carbon nanotubes available today. NC7000 carbon nanotubes have one of the most perfect chemical surfaces enabling high efficiency in the matrix in which they're embedded.NC7000 is available in powder form in quantities starting at 2 kg to multi-tons.Pre-dispersed forms are also available (PLASTICYL™, EPOCYL™, AQUACYL™)
Physical Properties Metric English Comments
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Specific Surface Area 250 - 300 m²/g
250 - 300 m²/g
BET
Mechanical Properties Metric English Comments
Tensile Strength 10000 - 60000 MPa
1.45e+6 - 8.70e+6 psi
Elongation at Break 10 %
10 %
Tensile Modulus 1000 GPa
145000 ksi
Thermal Properties Metric English Comments
Thermal Conductivity >= 3000 W/m-K
>= 20800 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C >= 90 %
>= 90 %
TGA
Electrical Properties Metric English Comments
Volume Resistivity 0.00001 - 0.0001 ohm-cm
0.00001 - 0.0001 ohm-cm
Descriptive Properties Value Comments
Amorphous Carbon Pyrolytically deposited carbon on the Surface of the NC7000
HRTEM
Average Diameter 9.5 nanometers
TEM
Average Length 1.5 microns
TEM
Metal Oxide 10% by TGA
TGA