Mateck CdSe

Category Other Engineering Material , Semiconductor
Manufacturer Mateck GmbH
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck CdSe.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semiconductor single crystals
Descriptive Properties Value Comments
Crystal Axis (0001)
Orientation (0001), (11-20), (10-10)
Orientation Accuracy ( ° ), Max 1
Polishing one side or both sides polished
Production Method Markov
Standard Size (mm) 10 x 10 x 0.5 or 1
Structure hexagonal