Material Notes:
Fibrelam® 5000 panels are lightweight, high performance structural sandwich panels that consist of cross-plied unidirectional fiberglass skins bonded to Aluminum honeycomb core. These panels exhibit superior mechanical and physical properties, are easy to install, and can be easily cut and machined on equipment normally found in airline maintenance shops. Fibrelam® 5000 panels are approved and qualified for use as flooring on Boeing aircraft.Information provided by Hexcel
Descriptive Properties Value Comments
Burn Length (mm) 28
BSS 7230; Flammability: 60 Second Vertical Ignition
Drip Extinguish Time (sec) 0
BSS 7230; Flammability: 60 Second Vertical Ignition
Glow Time (sec) 0
BSS 7230; Flammability: 45 Degree Test
In-Plane Shear (N/mm) 86
BMS 4-23
Insert Shear (N) 6140
BMS 4-23
Long Beam Bending Deflection (mm) 13
MIL-STD-401B; At 445N (100lb)
Long Beam Bending Load (N) 1220
BSS 7250 Humidity; Humidity Resistance Load (100% at 60°C (140°F) for 30 days)
1470
MIL-STD-401B; Core Ribbon, Transverse
Panel Shear Strength (N) 4890
MIL-STD-401B 3 point loading; Core Ribbon, Transverse
Sandwich Peel (N/76 mm) 410
MIL-STD-401B 3 point loading; Core Ribbon, Transverse
Self-Extinguish Time (sec) 0
BSS 7230; Flammability: 60 Second Vertical Ignition
1.4
BSS 7230; Flammability: 45 Degree Test
Stabilized Core Compression (N/mm2) 11.5
MIL-STD-401B
Warpage (mm/m), max 1.2