Material Notes:
Hexyltrichlorosilane fluidInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc

@Temperature 25.0 °C
1.10 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 2.0 cSt
2.0 cSt
Molecular Weight 219.6 g/mol
219.6 g/mol
Thermal Properties Metric English Comments
Boiling Point 191 °C
376 °F
Flash Point 84.0 °C
183 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance colorless