Dow Corning TM-4060 EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning TM-4060 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® TM-4060 Emulsion is specifically designed as a topical treatment for premium tissue softening in order to provide soft handle while maintaining the typical tissue water absorbency characteristics. Specific applications include premium facial, handkerchief and bath tissue, produced from virgin as well as recycled fibers. Dow Corning® TM-4060 Emulsion is particularly beneficial in the preparation of premium facial and bath tissue.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc

@Temperature 25.0 °C
1.00 g/cc

@Temperature 77.0 °F
Solids Content 30 %
30 %
pH 4.5 - 6.0
4.5 - 6.0
Kinematic Viscosity 40 cSt
40 cSt
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance hazy
Hydrophilic yes