Dow Corning SYL-OFF® SL 9151 RELEASE MODIFIER

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® SL 9151 RELEASE MODIFIER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-Off® SL 9151 Release Modifier is a solvent-free release coating for filmic pressure sensitive laminate/labelstock. Provides low temperature cure performance, suiteable for coating mono oriented polypropylene films and polyethylene coated kraft.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Kinematic Viscosity 1100 cSt
1100 cSt
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Appearance clear liquid
Solvent solventless