Dow Corning CB-1556 Fluid

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning CB-1556 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This fluid is a clear viscous liquid, where approximately 12% of an ultra high viscosity Dimethiconol gum is dispersed into phenyl functional silicone fluid.Areas of potential use for CB-1556 Fluid encompass a wide range of Cosmetic and Toiletry applications such as skin care, hair care, sun care, and color cosmetics.INCI NAME: Phenyl Trimethicone (and) DimethiconolInformation provided by Dow Corning
Physical Properties Metric English Comments
Viscosity Measure 5000 cSt
5000 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point >= 105 °C
>= 221 °F
Open cup
Optical Properties Metric English Comments
Refractive Index 1.452
1.452
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (%) <0.94
Nonvolatile Content (%) 100