Dow Corning 2-1352 EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-1352 EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 60% non-ionic emulsion of a blend of ultra-high molecular weight polydimethylsiloxane and high molecular weight polydimethylsiloxane for use in shower gels and hair care applications.Information provided by Dow Corning
Physical Properties Metric English Comments
pH 6.0
6.0
Descriptive Properties Value Comments
Active Content (%) 60
Non-Ionic yes