Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 1.70 g/cc
0.0614 lb/in³
Mechanical Properties Metric English Comments
Compressive Strength 29.4 MPa
4270 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Carbon, C 88 %
88 %