Beijing Evergrow Resources Polyurethane Activated Carbon

Category Carbon , Carbon Fiber
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources Polyurethane Activated Carbon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:good strengthgood flexilitygood durabilityApplications:Air purificationInformation provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Thickness 3000 - 30000 microns
118 - 1180 mil
Component Elements Properties Metric English Comments
Carbon, C 35 - 55 %
35 - 55 %
activated carbon
Descriptive Properties Value Comments
Air Resistance (Pa) 42
linear air speed: 1.0 m/s/hr; 4mm thickness
98
linear air speed: 1.0 m/s/hr; 27mm thickness
Toluene Adsorption 25-35%
Width (mm) 1000