PRODUCT NO. Category Trade Name
Plastics Group Polifil® RMT-30 30% Talc-Reinforced Polypropylene, High Impact Polypropylene with 30% Talc Filler Polifil®
Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene Polypropylene with 30% Talc Filler Polifil®