Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4000 A (Hot Water Moldable) Polyphthalamide (PPA)
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4000 A TFE 10 (Hot Water Moldable) Polyphthalamide (PPA), PTFE Lubricated
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4000 AFA-6145 V0 (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4001 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4001 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4002 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4002 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4003 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4003 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4005 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4005 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4007 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4007 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4008 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4008 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4009 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4009 A MS (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber Reinforced - Molybdenum Disulfide Lubricated
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4011 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4081 A (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4083 A (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4085 A (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4085 A TFE 15 (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4087 A (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4087 A FR (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4005.3 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4005.3 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4006 A FR Hot Water Moldable Polyphthalamide (PPA); Glass Fiber Reinforced - Flame Retardant