Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE COPEC® CC6OCZ Thermoplastic Elastomer, adhesion to ABS, PC and PC/ABS
The VS/AD1 Series is recommended for applications in the consumer electronics section. The compounds feature an exceptionally silky and velvety surface, accompanied by excellent adhesion properties ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE COPEC® CC7OCZ Thermoplastic Elastomer, adhesion to ABS, PC and PC/ABS
The VS/AD1 Series is recommended for applications in the consumer electronics section. The compounds feature an exceptionally silky and velvety surface, accompanied by excellent adhesion properties ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TC3GPN Thermoplastic Elastomer, General purpose
The GP/FG Series is recommended for a variety of different applications. It is particularly appropriate for passenger compartments. The compounds are available in natural and black colors. Typical a..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC3SCE Thermoplastic Elastomer, high scratch resistance
The SCR Series is recommended for applications requiring a high degree of scratch resistance. The series is characterized, among other things, by a pleasant feel. Typical applications: Car matsFunct..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC4PCN Thermoplastic Elastomer, Adhesion to PA, optimized compression set
The AD/PA/CS Series is recommended for applications with excellent adhesion to PA as well as outstanding compression set. The compounds are available in natural and black colors. Typical application..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TC5CSN Thermoplastic Elastomer, Optimized compression set
The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC5NYZ Thermoplastic Elastomer, Adhesion to PA
The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TC6FRN Thermoplastic Elastomer, Flame retardant
The FR Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Seals for..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC6NYN Thermoplastic Elastomer, Adhesion to PA
The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC6UVZ Thermoplastic Elastomer, UV resistance
The UV/AP Series is recommended for applications requiring high UV resistance. It is particularly suited for automotive exterior components. The compounds comply with GM standard GMW 16233. Typical ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC7PAN Thermoplastic Elastomer, Adhesion to PA
The AD/PA Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design elements..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC7PCZ Thermoplastic Elastomer, Adhesion to PA, optimized compression set
The AD/PA/CS Series is recommended for applications with excellent adhesion to PA as well as outstanding compression set. The compounds are available in natural and black colors. Typical application..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC7SCE Thermoplastic Elastomer, high scratch resistance
The SCR Series is recommended for applications requiring a high degree of scratch resistance. The series is characterized, among other things, by a pleasant feel. Typical applications: Car matsFunct..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC8MLZ Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC8NYN Thermoplastic Elastomer, Adhesion to PA
The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC8SCE Thermoplastic Elastomer, high scratch resistance
The SCR Series is recommended for applications requiring a high degree of scratch resistance. The series is characterized, among other things, by a pleasant feel. Typical applications: Car matsFunct..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TC9CSN Thermoplastic Elastomer, Optimized compression set
The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TC9FRZ Thermoplastic Elastomer, Flame retardant
The FR Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Seals for..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TP3CDZ Thermoplastic Elastomer, Adhesion to PP
The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TP5CDB Thermoplastic Elastomer, Adhesion to PP
The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TP7CDZ Thermoplastic Elastomer, Adhesion to PP
The EX Series is recommended for extrusion applications such as door seals and window gaskets. The compounds are available in natural and black colors. Typical applications: Edge guardsProfiles for ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® V TV6LVZ Thermoplastic Elastomer, General purpose, long term performance
The LTP Series is recommended for sealings requiring high temperature resistance. The compounds are characterized by an excellent adhesion to PP. Typical applications: FasteningsGrommetsSealsMateria..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TC6GPN Thermoplastic Elastomer, General purpose
The GP/FG Series is recommended for a variety of different applications. It is particularly appropriate for passenger compartments. The compounds are available in natural and black colors. Typical a..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TC7UVZ Thermoplastic Elastomer, UV resistance
The UV/AP Series is recommended for applications requiring high UV resistance. It is particularly suited for automotive exterior components. The compounds comply with GM standard GMW 16233. Typical ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TF4STE Thermoplastic Elastomer, optimized compression set
The FC/CS Series is recommended for applications with food contact providing an excellent compression set. The series is available in translucent colors. Typical applications: Closures Flexible Conn..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TF8BTL Thermoplastic Elastomer
The FC/AP Series is a natural-colored and translucent material solution for applications with food contact. The series’ features include excellent adhesion to PP. Typical applications: Function..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TP5NLZ Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA
The AD2 Series is recommended for applications with excellent adhesion to polar thermoplastics such as SAN, ASA, PMMA. The compounds are available in natural and black colors. Typical applications: ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TP5SKZ Thermoplastic Elastomer, Outdoor Grade
Typical applications of the EX/UV Series: Edge guardsDistance ProfilesMolded Parts (Solar Equipment)SealsInformation Provided by Kraiburg TPE Corp.
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Kraiburg TPE THERMOLAST® K TP6NLZ Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA
The AD2 Series is recommended for applications with excellent adhesion to polar thermoplastics such as SAN, ASA, PMMA. The compounds are available in natural and black colors. Typical applications: ..
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Kraiburg TPE THERMOLAST® K TF1SNT Thermoplastic Elastomer, very low rubber hardness
The FC/ht Series is a highly transparent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP. Typical applications:..