Processing Properties Metric English Comments
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1600FC PBT, Unfilled
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2008 PBT, Unfilled
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2300 GV1/20 PBT, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2300 GV1/30 PBT, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2300 GV3/20 PBT, 20% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2300 GV3/30 PBT, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3200-2 PBT, 15% Glass Reinforced
Celanex 3200-2 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3200-2 contains an internal lubricant.In..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3200FC PBT, 15% Glass Reinforced
Celanex 3200FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3216 PBT, 15% Glass Reinforced
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3300-2 PBT, 30% Glass Reinforced
Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3309HRT PBT, 30% Glass Reinforced
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 4306UV PBT, 30% Glass Reinforced
Celanex 4306UV is a 30% glass reinforced, toughened, low warpage, UV stable thermoplastic polyester.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese Celstran® PBT-GF40-08 PBT, 40% Glass Reinforced
40% Long Glass Fiber Reinforced PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 4602Z PBT, Unfilled
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 4612R PBT, 7% Glass Reinforced
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 4632Z PBT, 15% Glass Reinforced
Vandar 4632Z is a high impact, 15% glass reinforced polyester alloy. It combines high strength and toughness with a moderate degree of rigidity. It is characterized by excellent solvent resistance, ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3300-2LM PBT, Glass Reinforced
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release. It is a lasermarkable grade available i..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 531HS PBT, Glass Reinforced
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 6500 PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese IMPET 330R PET, 30% Glass Reinforced
Impet 330R is a 30% glass reinforced injection moldable polyester containing post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance...
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese RITEFLEX 425 TPC, Unfilled
Riteflex 425 is a nominal 25 Shore D thermoplastic polyester elastomer with low modulus and outstanding low temperature impact, and tear resistance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese RITEFLEX 640A TPC, Unfilled
40 Shore D Hardness 12,300 PSI flexural modulusInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 8000 PBT, Unfilled
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 2100 PBT, Unfilled
Vandar 2100 is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stabi..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 4302LM PBT, 30% Glass Reinforced
Celanex 4302LM is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.Information provided b..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 2122 PBT, 10% Mineral Reinforced
Vandar 2122 is a polyester alloy which contains 10% mineral filler. It offers exceptional toughness and practical impact strength. This resin offers Class A paintable finish with excellent dimension..