Polymer Property : Middle Barrel Temperature = 122 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1400FC PBT, Unfilled
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1600FC PBT, Unfilled
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1700A PBT, Unfilled
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1700FC PBT, Unfilled
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2000-3FC PBT, Unfilled
Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow mater..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2002 PBT, Unfilled
Celanex 2002 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002 ia a medium flow material.Information provide..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2300 GV3/30 PBT, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 2302 GV1/30 PBT, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3100-2 PBT, 7.5% Glass Reinforced
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.Information ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3216HR PBT, 15% Glass Reinforced
Celanex 3216HR is a flame retarded, hydrolysis resistant, 15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3309HRLM PBT, 30% Glass Reinforced
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. lIt is a asermarkable ..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3400 PBT, 40% Glass Reinforced
Celanex 3400 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding p..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3400-2 PBT, 40% Glass Reinforced
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3425HRT PBT, Glass Reinforced
Celanex 3425HRT is a non-lubricated, 40% fiberglass reinforced PBT copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.Information provided..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 4202 PBT, 15% Glass Reinforced
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese IMPET 2700 GV1/20 PET, 20% Glass Reinforced
Polyethylene terephthalate, 20 % glass fibre reinforced, high flowability, excellent gloss, high modulusInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 6035GB20 PBT, 20% Specialty
20% glass bead filled PBT.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese IMPET 2700 GV1/30 PET, 30% Glass Reinforced
30% glass filled Polyethylene terephthalate (PET) with high flowability, excellent gloss, high modulus, and high heat deflection temperature.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese RITEFLEX 435 TPC, Unfilled
Riteflex« 435 is a Thermoplastic Polyester Elastomer with a 35 nominal Shore D hardness, low modulus and outstanding low temperature impact strength and tear resistance.Information provided by Cela..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese RITEFLEX 655HS TPC, Unfilled
55 Shore D Hardness heat stabilizedInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese RITEFLEX 672 TPC, Unfilled
Riteflex 672 is a 72 Shore D Hardness thermoplastic polyester elastomer with a high modulus.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX J600 PBT, 40% Mineral / Glass Reinforced
Celanex J-600 is a 40% glass/mineral reinforced resin providing excellent warpage resistance, surface gloss and good mechanical properties. Celanex J-600 is particularly suited to applications requi..