Processing Properties Metric English Comments
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1400A PBT  (Unverified Data**)
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2000-3 PBT  (Unverified Data**)
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2002-3 PBT  (Unverified Data**)
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2404 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3300-2LM PBT, Glass Reinforced  (Unverified Data**)
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release.30% glass-filled PBT, laser markableInfo..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4302 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.30% glass-fiber, impact modifiedInformation provided by Celanese
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1662Z PBT, 30% Glass Reinforced
Celanex 1662Z is a 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processabilityTo avoid hydrolytic degradation during processing, CELANEX resins ha..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3226 PBT, Glass Reinforced
Celanex 3226 is a non-exuding, 20% glass-filled, flame retarded polybutylene terephthalate (PBT) which has an excellent balance of mechanical properties and processability. It is well suited for ele..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3314 PBT, 30% Glass Reinforced
Celanex 3314 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3409HR PBT, 40% Glass Reinforced
Celanex 3409HR is a non-lubricated, 40% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degra..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4302HS PBT, 30% Glass Reinforced
Celanex 4302HS is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance. Celanex 4302HS is ideally suited for heat shock applications such as ignition co..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 5202HF PBT, 15% Glass Reinforced
Celanex 5202HF is a 15% glass-filled polyester featuring improved surface gloss and high flow for long flow channels. A typical application is oven handles.Information provided by Celanese Corporat..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 5214HF PBT, 15% Glass Reinforced
Celanex 5214HF is a high flow, 15% glass reinforced, high gloss, flame retardant polyester.Pre-drying: 250F (120C) for 4 HoursInformation provided by Celanese Corporation.
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 7316 PBT, 35% Mineral / Glass Reinforced
Celanex 7316 is a non-exuding (UL and CSA approved V-0 at 1/32 inch), 35% glass/mineral reinforced PBT, which has an excellent balance of mechanical properties and processability. It is well suited..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3202-2 PBT, Glass Reinforced
Celanex 3202-2 is a 20% glass-filled Polybutylene Terephthalate that has an excellent balance of mechanical properties and processability. It contains an internal lubricant for mold release.To avoi..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3209HRT PBT, 15% Specialty
Celanex 3209HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate material that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celane..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced  (Unverified Data**)
30% long strand glass fiber reinforced thermoplastic polyurethane30% long strand glass fiber reinforced thermoplastic polyurethaneCelstran can be processed on a standard injection molding unit.Infor..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celstran® TPU-GF40-01-US TPU, 40% Glass Reinforced  (Unverified Data**)
40% long strand glass fiber reinforced thermoplastic polyurethane40% long strand glass fiber reinforced thermoplastic polyurethaneCelstran can be processed on a standard injection molding unit.Infor..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2000-3FC PBT  (Unverified Data**)
Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow mater..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3309HRT PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.30% glass reinforced, unlubricated, hy..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Average value: 255 °C Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese Corporation.