Processing Properties Metric English Comments
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2002-3 PBT  (Unverified Data**)
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2402 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2402 MT Natural is an unreinforced PBT with improved flow that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Master Fi..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2500 PBT  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: PBTBasic gradeInformation provided by Celanese
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.15% glass-fiber, improved impactInformation provided by Celanese
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4300FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.30% glass reinforced PBT for use in food contact applicationsInformation provided by Celanese
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4302 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.30% glass-fiber, impact modifiedInformation provided by Celanese
Hot-Working Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 5202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Vandar® 2500 PBT  (Unverified Data**)
Vandar 2500 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is specially designed to offer excellent chemical resistance, good colorability and dimensional ..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1662Z PBT, 30% Glass Reinforced
Celanex 1662Z is a 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processabilityTo avoid hydrolytic degradation during processing, CELANEX resins ha..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4302HS PBT, 30% Glass Reinforced
Celanex 4302HS is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance. Celanex 4302HS is ideally suited for heat shock applications such as ignition co..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 5214HF PBT, 15% Glass Reinforced
Celanex 5214HF is a high flow, 15% glass reinforced, high gloss, flame retardant polyester.Pre-drying: 250F (120C) for 4 HoursInformation provided by Celanese Corporation.
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Hot-Working Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 6407HR PBT, 30% Mineral / Glass Reinforced
Celanex 6407HR is a 30% glass/mineral reinforced hydrolysis resistant polyester particularly suited for large exterior automotive components where extended flow, flatness, and good surface appearanc..
Hot-Working Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 6500LM PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability, that is also enhanced for improved laser marking graphics.T..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3202-2 PBT, Glass Reinforced
Celanex 3202-2 is a 20% glass-filled Polybutylene Terephthalate that has an excellent balance of mechanical properties and processability. It contains an internal lubricant for mold release.To avoi..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3209HRT PBT, 15% Specialty
Celanex 3209HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate material that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celane..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3225HRT PBT, 15% Specialty
Celanex 3225HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at brea..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese Corpora..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3325HRT PBT, 30% Glass Reinforced
Celanex 3325HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at bre..
Hot-Working Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1400FC PBT  (Unverified Data**)
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3309HRT PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.30% glass reinforced, unlubricated, hy..
Hot-Working Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Hot-Working Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 6035GB20 PBT, 20% Glass Bead Filled
20% glass bead filled PBT.Information provided by Celanese Corporation.