Polymer Property : Processing Temperature = 93.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1400A PBT  (Unverified Data**)
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1600A PBT  (Unverified Data**)
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Extrusion gradeInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1700A PBT  (Unverified Data**)
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Highest molecular weightInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2001FC PBT  (Unverified Data**)
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2402 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2402 MT Natural is an unreinforced PBT with improved flow that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Master Fi..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300-2LM PBT, Glass Reinforced  (Unverified Data**)
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release.30% glass-filled PBT, laser markableInfo..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 4302 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.30% glass-fiber, impact modifiedInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 4309AR PBT  (Unverified Data**)
Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1400FC PBT, Unfilled
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2000-3FC PBT, Unfilled
Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow mater..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2001FC PBT, Unfilled
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2016 PBT, Unfilled
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2402 MT PBT, Medical Technology
Celanex 2402 MT Natural is an unreinforced PBT with improved flow that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Master Fi..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3216 PBT, 15% Glass Reinforced
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4300FC PBT, 30% Glass Reinforced
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4306UV PBT, 30% Glass Reinforced
Celanex 4306UV is a 30% glass reinforced, toughened, low warpage, UV stable thermoplastic polyester.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 1662Z PBT, 30% Glass Reinforced
Celanex 1662Z is a 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processabilityTo avoid hydrolytic degradation during processing, CELANEX resins ha..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3316 PBT, 30% Glass Reinforced
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4016 PBT, Unfilled
Non-exuding, unfilled, flame retardant polybutylene terephthalate which has an excellent balance of mechanical properties and processability. Celanex 4016 is well suited for applications requiring i..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 2003-3 PBT, Unfilled
Celanex 2003-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-3 is a medium h..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3209HRT PBT, 15% Specialty
Celanex 3209HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate material that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celane..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300D PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4306 PBT, 30% Glass Reinforced
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.Information provided by Celanese