Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 199 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1400A PBT  (Unverified Data**)
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1602Z PBT  (Unverified Data**)
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Lubricated extrus..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2016 PBT  (Unverified Data**)
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 2404 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3200-2FC PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3300-2 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 4300 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300 is a toughened, 30% glass reinforced PBT.30% glass-fiber, good impact strengthInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1400FC PBT, Unfilled
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1600A PBT, Unfilled
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1632Z PBT, 15% Glass Reinforced
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2002-2 PBT, Unfilled
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3216 PBT, 15% Glass Reinforced
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3309HRLM PBT, 30% Glass Reinforced
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability. lIt is a asermarkable ..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4300 PBT, 30% Glass Reinforced
Celanex 4300 is a toughened, 30% glass reinforced PBT.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4300FC PBT, 30% Glass Reinforced
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4306UV PBT, 30% Glass Reinforced
Celanex 4306UV is a 30% glass reinforced, toughened, low warpage, UV stable thermoplastic polyester.Information provided by Celanese
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.7.5% glass filledInform..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese Cor..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese Celanex® 3318 PBT, 30% Glass Reinforced
Celanex 3318 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
Cavity temperature
Celanese Celanex® 1600FC PBT  (Unverified Data**)
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Processing Temperature 65.0 - 93.0 °C
149 - 199 °F
cavity
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese
Copyright © lookpolymers.com All Rights Reserved