Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.317 W/m-K @Temperature 816 °C |
2.20 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C201 |
Thermal Ceramics TC-26 High Temperature Insulating Firebrick The bond developed is a ceramic bond that is formed by high temperature firing. This produces bricks that are very stable and strong at temperatures higher than 2600°F (1427°C). Features:High temp.. |
|||
Thermal Conductivity | 0.317 W/m-K @Temperature 538 °C |
2.20 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C201 |
Thermal Ceramics TC-26 HS High Temperature Insulating Firebrick The bond developed is a ceramic bond that is formed by high temperature firing. This produces bricks that are very stable and strong at temperatures higher than 2600°F (1427°C). Features:High temp.. |