Mechanical Properties Metric English Comments
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
73°F; ISO 180
Multibase Multi-Pro® 2502 CU Black Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Izod Impact, Notched 0.147 - 11.0 J/cm
0.276 - 20.6 ft-lb/in
Average value: 1.12 J/cm Grade Count:380
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Izod Impact, Notched 0.147 - 0.481 J/cm
0.276 - 0.900 ft-lb/in
Average value: 0.259 J/cm Grade Count:10
Overview of materials for Acrylic, High Flow, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched 0.147 J/cm
0.276 ft-lb/in
ASTM D256
Lendell Parapet PMMA, High Flow
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion
General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical EH910 PMMA, General Purpose Grade for Extrusion
Excellent solvent resistanceHighest of all grades in heat resistance, mechanical strength, surface hardness and stress cracking resistanceFeatures: Excellent transparency and eleganceWeather resista..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding
High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding
Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding
General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Izod Impact, Notched 0.147 J/cm
0.276 ft-lb/in
ASTM D256
E-Polymers SEPAZ® V200L Unfilled PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Izod Impact, Notched 0.147 - 0.588 J/cm
0.275 - 1.10 ft-lb/in
Average value: 0.309 J/cm Grade Count:10
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
ASTM D256
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..