Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 15000 - 50000 microns | 591 - 1970 mil | |
Microtherm Group Board Filament Reinforced Pyrogenic Silica Thermal Insulation Microtherm® Board is a high performance thermal insulation made at a lower density than normal Microtherm products. The insulation is an opacified blend of filament reinforced pyrogenic silica, s.. |
|||
Thickness | 6250 - 50000 microns | 246 - 1970 mil | |
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials |
|||
Thickness | 6250 - 50000 microns | 246 - 1970 mil | |
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials |
|||
Thickness | 6250 - 50000 microns | 246 - 1970 mil | |
Thermal Ceramics Cerablanket Blanket Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave.. |
|||
Thickness | 6250 - 50000 microns | 246 - 1970 mil | |
Thermal Ceramics Cerablanket Blanket Strip Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon .. |
|||
Thickness | 6250 - 50000 microns | 246 - 1970 mil | |
Thermal Ceramics Cerablanket Mesh Enclosed Rounds, Strips and Blankets Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w.. |
|||
Thickness | 12500 - 50000 microns | 492 - 1970 mil | |
Thermal Ceramics Cerachem Blanket Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe.. |
|||
Thickness | 12500 - 50000 microns | 492 - 1970 mil | |
Thermal Ceramics Cerachem Blanket Strip Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon .. |
|||
Thickness | 12500 - 50000 microns | 492 - 1970 mil | |
Thermal Ceramics Cerachem Mesh Enclosed Rounds, Strips and Blankets Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w.. |
|||
Thickness | 12500 - 50000 microns | 492 - 1970 mil | |
Thermal Ceramics Cerachrome Blanket Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg.. |
|||
Thickness | 3125 - 50000 microns | 123.0 - 1970 mil | |
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w.. |
|||
Thickness | 25000 - 50000 microns | 984 - 1970 mil | |
Thermal Ceramics Kaowool S Blanket Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F .. |
|||
Thickness | 12500 - 50000 microns | 492 - 1970 mil | |
Thermal Ceramics Kaowool S Blanket Strip Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon .. |
|||
Thickness | 3125 - 50000 microns | 123.0 - 1970 mil | |
Thermal Ceramics Kaowool Blanket Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens.. |