Physical Properties Metric English Comments
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachem Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachem Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thickness 12500 microns
492 mil
Thermal Ceramics Cerafiber® Wet Pack
Cerafiber Wet Pack is manufactured by combining Cerablanket®, a needled refractory fiber blanket, and inorganic binding agents. Cerafiber Wet Pack is packaged in moist form in polyethylene bags. It..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Kaowool S Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Thickness 12500 microns
492 mil
Thermal Ceramics Kaowool Wet Felt
Thermal Ceramics Kaowool Wet Felt is manufactured by combining Kaowool ceramic fiber with an inorganic bonding agent. It is very pliable with good green strength. Wet Felt may be cut into any size o..