Thickness 3125 microns
123.0 mil
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thickness 3125 microns
123.0 mil
Mid-Mountain Materials CERMEX® PR2200SW Thermal Insulation Mat
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thickness 3125 - 50000 microns
123.0 - 1970 mil
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Thickness 3125 - 50000 microns
123.0 - 1970 mil
Thermal Ceramics Kaowool Blanket
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens..