Polymer Property : Thickness = 246 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 6250 - 50000 microns
246 - 1970 mil
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thickness 6250 - 50000 microns
246 - 1970 mil
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thickness 6250 microns
246 mil
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thickness 6250 microns
246 mil
Mid-Mountain Materials CERMEX® PR2200SW Thermal Insulation Mat
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Ceramics Cerablanket Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Ceramics Cerablanket Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Thickness 6250 microns
246 mil
Thermal Ceramics Cerafiber® Wet Pack
Cerafiber Wet Pack is manufactured by combining Cerablanket®, a needled refractory fiber blanket, and inorganic binding agents. Cerafiber Wet Pack is packaged in moist form in polyethylene bags. It..
Thickness 6250 microns
246 mil
Thermal Ceramics Kaowool Wet Felt
Thermal Ceramics Kaowool Wet Felt is manufactured by combining Kaowool ceramic fiber with an inorganic bonding agent. It is very pliable with good green strength. Wet Felt may be cut into any size o..