Polymer Property : Thickness = 1970 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 15000 - 50000 microns
591 - 1970 mil
Microtherm Group Board Filament Reinforced Pyrogenic Silica Thermal Insulation
Microtherm® Board is a high performance thermal insulation made at a lower density than normal Microtherm products. The insulation is an opacified blend of filament reinforced pyrogenic silica, s..
Thickness 6250 - 50000 microns
246 - 1970 mil
Mid-Mountain Materials CERMEX® BK1800SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thickness 6250 - 50000 microns
246 - 1970 mil
Mid-Mountain Materials CERMEX® BK2200SW Low Biopersistence Thermal Insulation Blanket
Alkaline Earth Silicate Wool, Needled BlanketInformation provided by Mid-Mountain Materials
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Ceramics Cerablanket Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Thickness 6250 - 50000 microns
246 - 1970 mil
Thermal Ceramics Cerablanket Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachem Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachem Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thickness 3125 - 50000 microns
123.0 - 1970 mil
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Thickness 25000 - 50000 microns
984 - 1970 mil
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..
Thickness 12500 - 50000 microns
492 - 1970 mil
Thermal Ceramics Kaowool S Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Thickness 3125 - 50000 microns
123.0 - 1970 mil
Thermal Ceramics Kaowool Blanket
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens..