Polymer Property : Density = 0.184 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.144 - 0.184 g/cc
0.00521 - 0.00666 lb/in³
Range represents a tolerance from nominal of -10%/+15%.; ISO 845
DIAB Klegecell® R 200 Rigid, Closed Cell PVC Foam Core Material
Klegecell R is a PVC based, rigid, closed-cell foam with a tri-dimensional grid structure, which provides high thermal stability and structural integrity. As a structural core, Klegecell R is used i..