POLYMER SEARCH
Zoltek
Trade Name Panex 35®
Trade Name :
Panex 35®
Product List
Category
Carbon Fiber
,
Composite Fibers
,
Carbon Fiber/Thermoset Composite
,
Epoxy/Carbon Fiber Composite
Manufacturer
Zoltek
Tips:
50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO.
Category
Zoltek Panex 35® 50k Continuous Tow Commercial Carbon Fiber for Industrial Applications
Composite Fibers
Zoltek Panex 35® Carbon Felt
Composite Fibers
Zoltek Panex 35® Milled Carbon Fibers
Composite Fibers
Zoltek Panex 35® Stitch-Bonded Uni-Directional Carbon Fiber Fabrics
Composite Fibers
Zoltek Panex 35® Tow Weave Carbon Fiber Fabrics
Composite Fibers
Zoltek Panex 35® Type 48 Chopped Carbon Fiber
Composite Fibers
Zoltek Panex 35® Type 65 Chopped Carbon Fiber for Engineering Thermoplastic Applications
Composite Fibers
Zoltek Panex 35® Type 85 Chopped Carbon Fiber for High-Temperature Thermoplastics
Composite Fibers
Zoltek Panex 35® Uni-Directional Carbon Fiber Prepreg
Carbon Fiber/Thermoset Composite
Zoltek Panex 35® Unsized Chopped Fiber Flake
Composite Fibers
HOME
ABOUT US
POLYMER SEARCH
COMPANY NEWS
PRODUCT NEWS
CONTACT US
RFQ
Copyright © lookpolymers.com All Rights Reserved