Zircar Zirconia ZHB Zirconia Hollow Balls

Category Ceramic , Machinable Ceramic , Oxide , Zirconium Oxide
Manufacturer Zircar Zirconia
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Zirconia ZHB Zirconia Hollow Balls.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Zirconia Hollow Balls Type ZHB are sintered calcia-stabilized zirconia hollow balls, which flow easily into a confined space. Our standard product is our Type ZHB-1 which ranges in particle size from 0.2 mm to 3.0 mm diameter, which fill space effectively. They are useful for high temperature insulation in spaces where the insulation must be poured into place. The different size balls tend to segregate when poured as the larger balls tend to ‘float’ on top of the smaller balls. To minimize this effect, pour all the balls in at one time.Application Information: Zirconia Hollow Balls Type ZHB are useful as heat exchange media in fluidized bed reactors and as insulation in constrained spaces in very high temperature applications. The melting point of ZHB exceeds 4000°F. ZHB can be sieved into a more narrow size distribution on request.Information provided by Zircar Zirconia.
Physical Properties Metric English Comments
Specific Gravity 5.60 g/cc
5.60 g/cc
Bulk Density 1.50 g/cc
0.0542 lb/in³
Component Elements Properties Metric English Comments
Al2O3 <= 0.80 %
<= 0.80 %
CaO 3.0 - 4.0 %
3.0 - 4.0 %
Fe2O3 <= 0.10 %
<= 0.10 %
HfO2 1.0 - 2.0 %
1.0 - 2.0 %
SiO2 <= 0.60 %
<= 0.60 %
TiO2 <= 0.30 %
<= 0.30 %
ZrO2 >= 91 %
>= 91 %
Descriptive Properties Value Comments
Angle of Repose 30°
Color Yellow
Crystal Structure 80% Cubic, 20% Monoclinic