Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRA-BOND 872-7TN1 is a flexible thixotropic epoxy. The high viscosity and long worklife make this material easy to handle. Also, the high thermal conductivity makes this product ideal for electronic applications requiring stress relief. TRA-BOND 872-7TN1 is packaged in pre-mixed and frozen syringes. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 247500 cP

@Temperature 25.0 °C
247500 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Adhesive Bond Strength 2.41 MPa
350 psi
Lap shear, alum to alum, @ 25°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.800 W/m-K
5.55 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 100 °C
3.00 hour

@Temperature 212 °F
480 min

@Temperature 75.0 °C
8.00 hour

@Temperature 167 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Working Life hours 8
At 25°C