Zircar Zirconia YK-15 Yttria Knit Textile Insulation

Category Ceramic , Machinable Ceramic , Oxide
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Zirconia YK-15 Yttria Knit Textile Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Yttria (yttrium oxide - Y2O3) is typically used as a stabilizer for zirconia. It is offered here in its pure and stable metal oxide form, which is not attacked by most molten metals, including lithium and titanium. Our high purity yttria fiber and textiles are offered in six different standard product forms; bulk fiber Type YBF, two felts Types YF-50 and YF-100 and three types of knit cloth Types YK-15, YW-15 and YW-30.Features: High PurityHigh Temperature StabilityLow Thermal ConductivityExcellent Thermal Shock ResistanceNo OutgassingSix Different Product Formats OfferedAvailable ‘Off the Shelf’Application Information: Yttria textiles are used in the development of large grain Rare Earth Barium Copper Oxide (REBCO) melt processed high temperature superconductors (HTS).Information provided by Zircar Zirconia.
Physical Properties Metric English Comments
Bulk Density 0.420 g/cc
0.0152 lb/in³
Loss On Ignition 6.00 %

@Temperature 1650 °C,
Time 3600 sec
6.00 %

@Temperature 3000 °F,
Time 1.00 hour
Porosity 92 %
92 %
Bulk
Outgassing - Total Mass Loss 0.00 %
0.00 %
Thermal Properties Metric English Comments
Melting Point 2410 °C
4370 °F
Shrinkage 13.0 %

@Temperature 1650 °C,
Time 3600 sec
13.0 %

@Temperature 3000 °F,
Time 1.00 hour
Component Elements Properties Metric English Comments
Al2O3 0.0030 %
0.0030 %
Fe2O3 0.020 %
0.020 %
SiO2 0.020 %
0.020 %
Y2O3 >= 99 %
>= 99 %
Descriptive Properties Value Comments
Tensile Strength per Unit Width 18 gram/cm width