Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zircar Refractory Composites RS-ZIRGUARD ZIRCONIA COATING

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Zircar Refractory Composites, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Refractory Composites RS-ZIRGUARD ZIRCONIA COATING.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ZRCI Zirconium Oxide Coating Type RS-ZIRGUARD is a cream colored, water based paint of Zirconium Oxide (ZrO2). It is produced using high-purity, partially stabilized Zirconium Oxide (4 wt% CaO). It provides a high purity ceramic coating with utility to 1900°C (3452°F). It exhibits high chemical resistance and excellent release properties. Type RS-ZIRGUARD produces a hard, abrasion and chemical resistant coating that protects all ceramic bodies against most molten metals and corrosive environments, protecting them from spalling, dusting, and chemical attack. Type RS-ZIRGUARD may be applied to soft or fibrous structures to produce a more wear resistant surface layer which is also resistant to most high temperature reactions which may degrade the ceramic.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1900 °C
3450 °F
Component Elements Properties Metric English Comments
Other 10 %
10 %
ZrO2 90 %
90 %
Processing Properties Metric English Comments
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Color Cream
Coverage, ft2 100-400
Copyright © lookpolymers.com All Rights Reserved