Wieland Bio Porta 1020 Solder

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Silver Alloy , Solder/Braze Alloy
Manufacturer Wieland
Trade Name Bio Porta
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Bio Porta 1020 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solder supplied as strip (0.18 oz. roll)Information provided by WielandDental
Component Elements Properties Metric English Comments
Gold, Au 73.5 %
73.5 %
Silver, Ag 25 %
25 %
Zinc, Zn 1.5 %
1.5 %
Processing Properties Metric English Comments
Processing Temperature 1020 °C
1870 °F
Flow Temp
Melt Temperature 960 - 1010 °C
1760 - 1850 °F
Descriptive Properties Value Comments
Color yellow