Material Notes:
Designed for injection molding, extrusion, and blow moldingVery easy flowing grade for general useExcellent processability for multiple cavity moldsFeatures: Excellent strengthGood temperature resistanceApplications: Electronics packaging and office accessoriesAudio and Video componentsInformation provided by Dax Resinas
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 060
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa
7110 psi
ASTM D638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 3.17 GPa
460 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
@ 264 psi; ASTM D648
Vicat Softening Point 106 °C
223 °F
ASTM D1525
Flammability, UL94 HB
HB